⭐In Stock, Priority is given to delivery after payment.
⭐Returns>> Fast Refund, Money-Back Guarantee.
📧Contact Us: support@opportunuity.com.
The Strongest, Fastest, and Easiest Aluminum Fabrication or Parts Repair– no expensive equipment required.
1. Thoroughly clean the area you’re about to weld by brushing the base with stainless steel brush until it becomes shiny.
2. Then evenly heat the area to be welded.
3. As you heat, rub the rod vigorously against the heated area until the rod starts flowing.
![]()
Caution: Never apply heat directly to the rod as it will crumb, and if you manage to melt the rod directly, the weld will be easily breakable. Remember, melting the rod directly is a wrong way, and makes crumby welds.